当前位置: 产品展示
| 合金牌号 Brazing Alloy |
化学成分(%) Composition(%) |
Melting Range (°C) |
特性与应用 Principal areas of application | ||||
| Cu | P | Sn | 杂质总量 Impurities Total |
固相线 Solidus |
夜相线 Liquidus | ||
| HAg-2B | 余 | 1.8-2.2 | 6.8-7.2 | <0.10 | 645 | 790 | 有好的流动性和填充能力,广泛用于空调、冰箱、机电等行业,铜及铜合金的钎焊。 Widely used in brazing copper and copper alloy in the fields of air-conditioning and mechanical-electrical good flow property and filling capability |
| HAg-5B | 4.8-5.2 | 5.8-6.7 | 645 | 815 | 有一定塑性,适用不能保持紧密配合的铜及其合金接头的焊接。 Have certain Plasticity,suitable for brazing copper alloy and some copper,which can't conjugate tightly. | ||
| HAg-58C | 4.8-5.2 | 6.6-7.2 | 620 | 660 | 熔点低、工艺好、钎料可溶入极小缝隙,目前适用于对空调四通阀的钎焊。 Low melting point good technics,and it can dissolve into gap. | ||
| HAg-6B | 5.8-6.2 | 6.8-7.85 | 645 | 725 | 熔点低、特别适用自动钎焊,已大量用于四通阀与截止阀的焊钎。 It is of low melting point. It is especially fit for the automatic braze welding . It has been largely applied in the soldering with four-way valve and cut-off valve. | ||
| HAg-15B | 14.5-15.5 | 4.8-5.3 | 645 | 800 | 接头塑性,导电性提高,特别适用间隙不均场合。可钎焊承受振动载荷的铜及其合金接头的钎焊。 Bettered plasticity And conductivity of JOint,suitable especially for brazing copper and Copper alloy with Vibration load. | ||